Figure 1.

DSC trace and X-ray diffraction patterns. DSC trace of the studied amorphous Ti-Ni-Si alloy scanned at 0.67 K/s (a) and X-ray diffraction patterns of the studied alloy before and after de-alloying and then anodic oxidation (b).

Fukuhara and Sugawara Nanoscale Research Letters 2014 9:253   doi:10.1186/1556-276X-9-253
Download authors' original image