Table 4

The parameters of porous and fractal structure of PCM modified at 600°C
tmod (h) Q (nm−3) Kp (nm−4) ρm (g/сm3) w Sn (m2/g) Rp (nm) Rс (nm) rc (nm) Dv Ds
0 2,502 1,640 0.71 0.76 529 1.9 - - 2.4 2.6
0.25 2,496 1,740 0.58 0.71 777 1.8 16 2.0 - 2.6
0.5 2,553 1,780 0.56 0.72 788 1.8 15 2.5 - 2.55
0.75 2,584 1,950 0.56 0.72 853 1.7 15 2.5 - 2.6
1 2,482 1,860 0.56 0.72 847 1.7 15 2.0 - 2.6

Ostafiychuk et al.

Ostafiychuk et al. Nanoscale Research Letters 2014 9:160   doi:10.1186/1556-276X-9-160