Table 2

Variation in peak intensities measured from XRD diffractograms of thin (100 nm) ZnO NW arrays
ZnO peak 300 K (room temperature) 473 K 673 K 873 K
Intensity Relative intensity Intensity Relative intensity Intensity Relative intensity Intensity Relative intensity
100 114.7 0.02 155.1 0.03 257.4 0.1 312.1 0.13
002 119.4 0.03 162.7 0.06 248.8 0.07 261.8 0.11
101 264 0.03 389.8 0.06 460.0 0.25 623.6 0.26