Table 1

Variation in peak intensities measured from XRD diffractograms of ultrathin (15 nm) ZnO NW arrays
ZnO peak 300 K (room temperature) 473 K 673 K 873 K
Intensity Relative intensity Intensity Relative intensity Intensity Relative intensity Intensity Relative intensity
100 190.0 0.24 254.1 0.39 264.9 0.4 279.2 0.47
002 211.5 0.26 254.0 0.45 346.9 0.63 357.9 0.68
101 342.5 0.64 451.1 0.72 530.9 0.85 569.9 1.22

Shrama et al.

Shrama et al. Nanoscale Research Letters 2014 9:122   doi:10.1186/1556-276X-9-122