Figure 7.

XRD diffractogram of electrochemically grown approximately 100-nm ZnO nanowire arrays. (a) As grown (300 K). (b) UHV-annealed at 473 K. (c) UHV-annealed at 673 K. (d) UHV-annealed at 873 K.

Shrama et al. Nanoscale Research Letters 2014 9:122   doi:10.1186/1556-276X-9-122