Figure 6.

XRD diffractogram of electrochemically grown ZnO nanowire arrays at approximately 15 nm. (a) XRD of as-grown (300 K). (b) UHV-annealed at 473 K. (c) UHV-annealed at 673 K. (d) UHV annealed at 873 K.

Shrama et al. Nanoscale Research Letters 2014 9:122   doi:10.1186/1556-276X-9-122