Figure 7.

Photocurrent-voltage curves of TiO2nanofiber cells (sintered at 550°C and approximately 60-μm thick). With ZnO layer of different thicknesses (4 to 20 nm).

Ding et al. Nanoscale Research Letters 2013 8:9   doi:10.1186/1556-276X-8-9