Resolution: standard / high Figure 3.
EBSD phase maps. Illustrations of phase discrimination were obtained for the surface region of samples
(a) Cu/Si (100), (b) Cu/PS/Si (100), (c) Cu/Si (111), and (d) Cu/PS/Si (111).
Bandarenka et al. Nanoscale Research Letters 2013 8:85 doi:10.1186/1556-276X-8-85 |