Figure 3.

SiNWs grown at 200°C from (a) 100, (b) 40 and (c) 7.5nm Ga catalyst layers. The scale bar is1 μm.

Gabrielyan et al. Nanoscale Research Letters 2013 8:83   doi:10.1186/1556-276X-8-83
Download authors' original image