Figure 6.

Planar TEM images of ALD Pt on Al2O3 film. Corresponding to (a) 70 cycles, together with an electron diffraction image of selected area, and (b) 90 cycles.

Ding et al. Nanoscale Research Letters 2013 8:80   doi:10.1186/1556-276X-8-80