Resolution: standard / high Figure 9.
Temperature variations for deionized water and aqueous dispersions of Cs0.33WO3 nanoparticles with NIR irradiation time. Cs0.33WO3 nanoparticles were obtained after grinding for 3 h. Their concentrations ranged from
0.008 to 0.4 wt.%.
Chen and Chen Nanoscale Research Letters 2013 8:57 doi:10.1186/1556-276X-8-57 |