Figure 10.

Temperature variation for aqueous dispersions of Cs0.33WO3 nanoparticles with NIR irradiation time for 5 cycles. Cs0.33WO3 nanoparticles were obtained after grinding for 3 h, and their concentration in the aqueous dispersions was 0.08 wt.%.

Chen and Chen Nanoscale Research Letters 2013 8:57   doi:10.1186/1556-276X-8-57