Figure 4.

SEM images of structures before and after annealing at 160°C for 24 h. Au/TPP/glass (A, B), Au/TPP/Au/glass (C, D), and Au/glass (E, F).

Kalachyova et al. Nanoscale Research Letters 2013 8:547   doi:10.1186/1556-276X-8-547