Figure 8.

Trajectories of the magnetization at the top of the hard section for the ECC grain. Projected onto the x-z plane under the field conditions (a)Hdc = 16.6 kOe, Hac = 0.5 kOe and (b)Hdc = 11.4 kOe, Hac = 0.6 kOe at 0 K. The dc field incident angle is 0°.

Tanaka et al. Nanoscale Research Letters 2013 8:461   doi:10.1186/1556-276X-8-461