Figure 5.

Measured reflectivity of fabricated PC film and bare PC film. Fabricated PC film with various depths of nanoinjected submicron holes and bare PC film as a function of the wavelengths. The mirror means the bare PC film, while the numbers of 115 to 130 corresponds to the molding temperatures in Celsius and associated depths can be referred to Figures 4 and 6, respectively.

Fuh et al. Nanoscale Research Letters 2013 8:407   doi:10.1186/1556-276X-8-407