Figure 6.

TEM images of samples after self-limiting oxidation. (a) to (f) TEM images of samples after 10-h self-limiting oxidation at (a) 750°C, (b) to (e) 800°C, and (f) 850°C.

Su et al. Nanoscale Research Letters 2013 8:405   doi:10.1186/1556-276X-8-405