Figure 9.

Rheological measurements of pristine MEH-PPV and CdS/MEH-PPV nanocomposites. With a weight/weight ratio between precursor and polymer of 1:4 carried out at 200°C.

Laera et al. Nanoscale Research Letters 2013 8:382   doi:10.1186/1556-276X-8-382