Figure 7.

TEM images of CdS/MEH-PPV nanocomposites. Obtained at 185°C starting from a solution with a weight/weight ratio precursor/polymer of 1:4 (a, b) and from a solution with a weight/weight ratio precursor/polymer of 2:3 (c, d).

Laera et al. Nanoscale Research Letters 2013 8:382   doi:10.1186/1556-276X-8-382