Figure 4.

PL spectra of CdS NCs. In MEH-PPV (a) and in PMMA (b) grown at 175°C and 185°C (excitation wavelength 330 nm), respectively.

Laera et al. Nanoscale Research Letters 2013 8:382   doi:10.1186/1556-276X-8-382