Resolution: standard / high Figure 1.
TEM images and XRD data of TiO2 nanorods after sintering at various temperatures. (a) 450°C, (b) 650°C, (c) 750°C, (d) 850°C, (e) 1,000°C, and (f) XRD.
Jung et al. Nanoscale Research Letters 2013 8:37 doi:10.1186/1556-276X-8-37 |