Figure 11.

The process of phase transformation in nanoindentation on the (010) germanium surface. The indentation depth is (a) approximately 1.2 nm, (b) approximately 2 nm, and (c) approximately 4.5 nm.

Lai et al. Nanoscale Research Letters 2013 8:353   doi:10.1186/1556-276X-8-353