Figure 4.

XRD patterns of deposited Au/PSi. Samples were deposited using different current densities of (a) 1.5, (b) 2.5, (c) 3.5, and (d) 4.5 mA/cm2, respectively, (A) for the range 2θ = 37° to 39° and (B) for the range of 2θ = 60° to 90°.

Amran et al. Nanoscale Research Letters 2013 8:35   doi:10.1186/1556-276X-8-35