Figure 2.

Cross-sectional TEM image of the sol–gel-derived TixZrySizO film. The thickness of the TixZrySiz O film is calculated to be 2 nm after 600°C annealing.

Chang et al. Nanoscale Research Letters 2013 8:340   doi:10.1186/1556-276X-8-340