Figure 5.

I-V curves. For bare Si solar cell and Si solar cells coated with QD-doped PLMA at CQD = 0 and 1.6 mg/ml.

Cheng et al. Nanoscale Research Letters 2013 8:291   doi:10.1186/1556-276X-8-291