Figure 5.

TGA of pristine and PEI-functionalized carbon nanotubes. The amount of PEI introduced to PEI-NH-SWNTs (A) or PEI-NH-MWNTs (B) during the functionalization procedure was quantified by the additional weight loss of PEI-NH-SWNTs and PEI-NH-MWNTs at 420°C compared to pristine carbon nanotubes.

Huang et al. Nanoscale Research Letters 2013 8:267   doi:10.1186/1556-276X-8-267