Table 1

Increase of pore diameters in Ag-MNP-containing Purolite C100E resin samples
Sample Ag-MNP content (mg/g) BET average pore diameter (nm)
C100E 0 1.9
Ag-C100E PMNC (5a) 112.7 ± 0.5 2.3 ± 0.2
Ag-C100E PMNC (10a) 143.5 ± 0.5 4.4 ± 0.2

aNumbers show the time of metal loading cycle carried out.

Bastos-Arrieta et al.

Bastos-Arrieta et al. Nanoscale Research Letters 2013 8:255   doi:10.1186/1556-276X-8-255