Figure 1.

Dependence of Au layer sheet resistance of evaporated samples deposited on glass at different temperatures. The dependence of Au layer sheet resistance on the layer thickness measured for evaporated samples deposited on glass at room temperature (RT), deposited on substrate heated to 300°C (300°C) and deposited on glass with room temperature and consequently annealed at 300°C (annealing).

Schaub et al. Nanoscale Research Letters 2013 8:249   doi:10.1186/1556-276X-8-249