Table 1

Photovoltaic characteristics of SCNTs-Si solar cell for SCNT immersion in Au solution at different times
Time (min) JSC (mA/cm2) Voc (V) FF (%) PCE (%) Rs (Ω cm2) Carrier density (cm−2)
0 5.2 ± 0.05 0.38 ± 0.02 18 ± 0.01 0.36 ± 0.06 8.72 ± 0.01 5.3 × 1018
10 7.2 ± 0.04 0.45 ± 0.01 26 ± 0.01 0.84 ± 0.04 7.5 ± 0.02 7.9 × 1019
20 7.65 ± 0.06 0.50 ± 0.02 30 ± 0.02 1.15 ± 0.05 5.84 ± 0.01 1.4 ×1020
30 7.46 ± 0.05 0.47 ± 0.01 31 ± 0.01 1.09 ± 0.04 5.65 ± 0.02 1.3 × 1021
40 7.1 ± 0.02 0.46 ± 0.02 30 ± 0.01 0.98 ± 0.01 5.63 ± 0.02 1.5 × 1021

Chen et al.

Chen et al. Nanoscale Research Letters 2013 8:225   doi:10.1186/1556-276X-8-225

Open Data