Figure 7.

Nanoindentation MD simulation load-displacement curves on the machining-induced surface and pristine single-crystal copper. The indenter radius is 5.0 nm, and the maximum penetration depth is 2.5 nm.

Zhang et al. Nanoscale Research Letters 2013 8:211   doi:10.1186/1556-276X-8-211