Figure 12.

Hysteresis loops measure at various temperatures. Hysteresis loops (a) measured at 10 K for Si nanowires Mn+-implanted to doses of 1 × 1015, 5 × 1015, 1 × 1016, and 2 × 1016 cm-2 and (b) taken at 10, 77, and 300 K for Si nanowires Mn+-implanted to a dose of 2 × 1016 cm-2. Reprinted with permission from Wu et al. [61].

Li et al. Nanoscale Research Letters 2013 8:175   doi:10.1186/1556-276X-8-175