Figure 3.

XPS depth profile of Fe-Al film oxidized for 20 min at 900°C. (TAnneal = 900°C, TDew = -17°C, and t = 20 min).

Jang et al. Nanoscale Research Letters 2013 8:152   doi:10.1186/1556-276X-8-152