Figure 7.

Micrograph of 25-nm-wide lifted-off Cr gratings. The metallization (50-nm thickness) was performed by e-beam evaporation.

Mohammad et al. Nanoscale Research Letters 2013 8:139   doi:10.1186/1556-276X-8-139
Download authors' original image