Figure 6.

Comparison of the hillocks produced with different diamond tips under the same contact pressure. (a) R = 500 nm; (b) R = 250 nm. The number of scratch cycles was 100.

Yu and Qian Nanoscale Research Letters 2013 8:137   doi:10.1186/1556-276X-8-137