Table 1

Electrochemical parameters for each nucleant layer used
Nucleant layer Potentiostatic Galvanostatic Pulsed current
E (V) Time (s) I (mA) Time (s) I (mA) tON (s) tOFF (s) Time (s)
ITO −1 600 −4 600 −4 1 1 1,200
Spin-coated ZnO −1 600 −1.75 600 −1.75 1 1 1,200
Sputtered ZnO −0.8 600 −1.5 600 −1.5 1 1 1,200

Tolosa et al.

Tolosa et al. Nanoscale Research Letters 2013 8:135   doi:10.1186/1556-276X-8-135