Figure 14.

Permeances of helium at different temperatures using the same membrane. Permeances at 25°C (T01), at 25°C but after an exposure at 100°C (T02), and the same membrane after an exposure at 200°C (T03).

El Korhani et al. Nanoscale Research Letters 2013 8:121   doi:10.1186/1556-276X-8-121
Download authors' original image