Table 2 |
|||||||
|
Effect of different modifications of AAO pores on fringe intensity |
|||||||
|
Coating material |
AAO |
Pt |
Au |
Cr |
Ni |
Ag |
TiO2 (ALD) |
|
|
|||||||
|
Thickness (nm) |
8 |
8 |
9 |
5 |
13 |
10 |
|
|
Interference maximum intensitya (a.u.) |
10 ± 3 |
50 ± 5 |
98 ± 6 |
100 ± 8 |
65 ± 2 |
35 ± 2 |
11 ± 2 |
|
|
|||||||
|
aAverage of five measurements plus standard deviation. AAO, anodic aluminium oxide; ALD, atomic layer deposition; a.u., arbitrary unit. |
|||||||
|
Kumeria and Losic Nanoscale Research Letters 2012 7:88 doi:10.1186/1556-276X-7-88 |
|||||||