Figure 3.

Effects of adding ultrafine active alumina on the cold crushing strength of the castables. The castables were subjected with different amounts of Cr2O3 at temperatures of 110°C and 1,600°C.

Zhao et al. Nanoscale Research Letters 2012 7:8   doi:10.1186/1556-276X-7-8