Resolution: standard / high Figure 2.
XRD patterns of samples prepared at 200°C for 10 h under different calcination temperatures. (a) 200°C for 3 h, (b) 300°C for 3 h, and (c) 400°C for 3 h.
Shin et al. Nanoscale Research Letters 2012 7:73 doi:10.1186/1556-276X-7-73 |