Figure 2.

XRD patterns of ZnO films. (A) Not sintered and (B) sintered at 400°C for 1 h. The asterisk denotes the FTO substrate.

Chang et al. Nanoscale Research Letters 2012 7:688   doi:10.1186/1556-276X-7-688