AFM images of the samples: (a) initial glass surface; (b) glass surface after the
first anneal; (c) the profiles of bigger (1) and smaller (2) islands measured along
lines 1 and 2 in image (b); the widths of maxima correspond to the particles size;
(d) another region of the glass surface; (e) glass surface after 9 cycles of ‘removal-anneal’.