Resolution: standard / high Figure 6.
Bending test and in-situ measured resistance. (a) The pictures of the bending test steps and (b) variation of the in-situ measured resistance ((R1-R0)/R0) during repeated bending cycles for R2R-sputtered IZO/Ag/IZO/Ag multilayer electrodes,
with inset optical microscope images of the top IZO layer before and after the bending
test.