Figure 6.

Bending test and in-situ measured resistance. (a) The pictures of the bending test steps and (b) variation of the in-situ measured resistance ((R1-R0)/R0) during repeated bending cycles for R2R-sputtered IZO/Ag/IZO/Ag multilayer electrodes, with inset optical microscope images of the top IZO layer before and after the bending test.

Kim and Lim Nanoscale Research Letters 2012 7:67   doi:10.1186/1556-276X-7-67