Resolution: standard / high Figure 1.
XRD patterns of PMNT/ZnO ceramics sintered at 1,150°C and XRD peak at 2θ ≈ 45°. The figure on the left showed XRD patterns of PMNT/xZnO ceramics, where x = 0, 0.05, 0.1, 0.5, and 1 wt.% of CuO measured from an angle range of 10° to 60°.
The other on the right showed a detail observation at angle ≈45° which indicated the
shifting of a peak with ZnO additions.
Promsawat et al. Nanoscale Research Letters 2012 7:65 doi:10.1186/1556-276X-7-65 |