Figure 4.

Raman spectra of CdS thin films deposited at RT and annealed at different temperatures. Inset image is the normalized intensity vs. Raman shift of 1LO mode.

Kumar et al. Nanoscale Research Letters 2012 7:584   doi:10.1186/1556-276X-7-584