Resolution: standard / high Figure 3.
GAXRD pattern of CdS thin films deposited at substrate temperature 200°C and annealed
at different temperatures.
Kumar et al. Nanoscale Research Letters 2012 7:584 doi:10.1186/1556-276X-7-584 |