Resolution: standard / high Figure 2.
Thermal conductivity of large-diameter SiNWs (approximately 350 nm; 1014cm−3p-type doping). The thermal conductivity with three levels of porosity, corresponding to different
etching conditions, is shown. The thermal conductivity decreases significantly with
increasing porosity. The inset images show the top view of the SiNWs, and the scale
bars are 200 nm.
Weisse et al. Nanoscale Research Letters 2012 7:554 doi:10.1186/1556-276X-7-554 |