Figure 1.

FTIR of as-deposited sample and RTA treated at 950°C. The blue arrow indicates the shift in the TO3 peaks of the two samples.

Saxena et al. Nanoscale Research Letters 2012 7:547   doi:10.1186/1556-276X-7-547