Table 2

OSC at 600 ° C of the Ce 0 .5 Zr 0 .4 Al 0 .1 O 1 .95 , Ce 0 .5 Zr 0 .2 Al 0 .3 O1 .85 , and Ce 0 .5 Zr 0 .1 Al 0 .4 O 1 .8 calcined at 1 , 000 ° C for 20 h
Chemical composition OSC (μmol-O g 1 )
Ce0.5Zr0.4Al0.1O1.95 378.0
Ce0.5Zr0.2Al0.3O1.85 389.0
Ce0.5Zr0.1Al0.4O1.8 261.0

Dong et al.

Dong et al. Nanoscale Research Letters 2012 7:542   doi:10.1186/1556-276X-7-542

Open Data