| OSC at 600 ° C of the CeO 2 , Ce 0 .5 Zr 0 .5 O2 , and Ce 0 .5 Zr 0 .3 Al 0 .2 O 1 .9 calcined at 1 ,000 ° C for 20 h | |
| Chemical composition | OSC (μmol-O g − 1 ) |
| CeO2 | 25.0 |
| Ce0.5Zr0.5O2a | 350.0 |
| Ce0.5Zr0.3Al0.2O1.9 | 427.0 |
aIt is accepted that the Ce0.5Zr0.5O2 composition possessed excellent OSC property [10-14].