Resolution: standard / high Figure 4.
Mn L2,3X-ray absorption. (a) XAS for magnetization and helicity parallel (μ+) and antiparallel (μ−) and (b) XMCD (μ + − μ−) measured at around 10 K under an external field of 6,000 Oe applied
perpendicular to the surface.
Zhou et al. Nanoscale Research Letters 2012 7:528 doi:10.1186/1556-276X-7-528 |